Basell Pro-fax™ KF6190H Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Pro-fax™ KF6190H, polypropylene homopolymer resin is designed for BOPP (biaxially oriented polypropylene) film extrusion applications, where good metallization is required. Pro-fax™ KF6190H resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Bi-axially oriented film, packaging Information provided by Basell.
|
|
|