Basell Pro-fax™ PDC 1267 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ PDC 1267 high melt flow polypropylene homopolymer resin is designed for fiber spinning applications that require resistance to gas fading. Pro-fax™ PDC 1267 resin meets FDA requirements in the Code of Federal Regulations, 21 CFR 177.1520 for food contact up to a temperature of 212 0F. All ingredients in Pro-fax™ PDC 1267 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Fibers, BCF yarn Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
|
|
|
|
| Property Data |