Basell Pro-fax™ PDC 1280 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Pro-fax™ PDC 1280 general purpose polypropylene homopolymer resin is suitable for strap, tape and film fiber applications. Pro-fax™ PDC 1280 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Strapping, tape, twine Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |