Basell Pro-fax™ PDC1307 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Pro-fax™ PDC1307, a high melt flow polypropylene homopolymer resin, is suitable for cast film extrusion. Pro-fax™ PDC1307 meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients in Pro-fax™ PDC1307 meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Cast film, fibers Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|