Basell Pro-fax™ SA933 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ SA933 super-high impact polypropylene copolymer resin is designed for general extrusion or injection molding equipment. Pro-fax™ SA933 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, excluding cooking applications. All ingredients in meet the chemical registration requirements of TSCA (US) and DSL (Canada). Uses: Automotive applications Information provided by Basell.