Basell Pro-fax™ SC204 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ SC204 polypropylene copolymer resin is designed for thermoforming and sheet extrusion applications. It is nucleated and features antistatic properties. Pro-fax™ SC204 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients in Pro-fax™ SC204 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Sheet, containers, thermoformed containers Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|