Basell Pro-fax™ SC-873 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ SC-873 fully formulated (antistatic, nucleated, slip modified), very high melt flow, medium impact polypropylene copolymer resin is designed for injection molding applications. This resin exceeds the performance of competitive grades by offering a good balance of properties with faster cycling capability. Other features include minimum warpage, good impact resistance at low temperatures, excellent gloss, and a good stiffness/impact balance. Pro-fax™ SC-873 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, excluding cooking applications. All ingredients of Pro-fax™ SC-873 meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Typical applications include consumer goods and housewares. Uses: Household goods, consumer applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|