Basell Pro-fax™ SD375S Polypropylene Copolymer

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Description: Pro-fax™ SD375S medium impact polypropylene copolymer resin is available in flake form. Flake form resin is well suited for mixing with pigments and other additives to make polymer concentrates or masterbatches. This resin has very minimal stabilization, which allows wide design latitude for the compounder. Additional suitable stabilization is required to protect the resin during melt processing and throughout its useful life. This resin is designed for applications requiring an excellent balance of stiffness and impact resistance. Pro-fax™ SD375S flake resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, excluding cooking applications. Please note that any additives compounded into this resin will require a re-assessment of its FDA status. All ingredients in Pro-fax™ SD375S resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Compounding, color concentrates

Information provided by Basell.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Impact
  • Izod Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。