Basell Pro-fax™ SG722 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ SG722 high flow, high impact polypropylene copolymer resin is designed for injection molding applications. This resin is available in pellet form. Pro-fax™ SG722 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520, for food contact, including cooking applications. All ingredients in Pro-fax™ SG722 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Household goods, toys, consumer applications, sporting goods Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|