MRC Polymers NAXALOY™ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled
Subcategory: Polycarbonate; Polyester, TP; Thermoplastic
Material Notes: 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Dew Point
- Drying Air Flow Rate
- Injection Pressure
- Back Pressure
- Cushion
- Screw Speed
- Fill Rate
- Hold Pressure
- Packing Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|