MRC Polymers NAXELL™ PC100H General Purpose Polycarbonate, High MFR
Subcategory: Polycarbonate; Thermoplastic
Material Notes:
- High Quality, High melt PC
- MFR can be modified between 10 to 40 g/10min
- Can be UV Stabilized
- Internal and external lubricant can be added
- Can be clear to color matched
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Transmission, Visible
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Dew Point
- Drying Air Flow Rate
- Injection Pressure
- Back Pressure
- Cushion
- Screw Speed
- Fill Rate
- Hold Pressure
- Packing Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|