Multibase Multi-Flex® TPE A 2504LC Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodFoamableHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Good Forms: PelletsProcessing Method: Extrusion Information provided by Multibase
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Tear Strength
- Compression Set
- Melt Temperature
|
|
|
|
| Property Data |