Multibase Multi-Flex® TPE A 7727 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good Forms: PelletsProcessing Method: Injection Molding Uses: Automotive Interior PartsInformation provided by Multibase
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tear Strength
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
- Screw Speed
- Clamp Tonnage
- Injection Rate
- Suggested Max Regrind
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|