Multibase Multi-Flex® TPE D 4201 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant General Purpose Forms: PelletsProcessing Method: Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation provided by Multibase
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Tear Strength
|
|
|
|
| Property Data |