Multibase Multi-Flex® TPE RP 6568 Styrene Ethylene Butylene Styrene Block Copolymer
Subcategory: Thermoplastic
Material Notes:
Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms: PelletsProcessing Method: Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation provided by Multibase
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
|
|
|
|
| Property Data |