Multibase Multi-Pro® Polypropylene 3019 CXUW
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Calcium Carbonate Filler, 30% by weight.Features: Gloss, High Impact Resistance, GoodUV Resistance, Good Forms: PelletsProcessing Methods: Injection MoldingUses: FurnitureLawn EquipmentInformation provided by Multibase
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
- Screw Speed
- Clamp Tonnage
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|