Custom Resins Nylene® NX4702 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Film Grade. Nylene NX4702 is an anti-static, extrusion grade nylon 6 resin suitable for blown or cast film applications. It has excellent melt flow, melt strength properties, and optical clarity. Nylene
NX4702 has superior grease resistance, toughness, resistance to abrasion, and does not
absorb food odors. Optimum processing conditions should provide a melt temperature of 525 -
540ºF at the die.
| Available Properties |
- Density
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Secant Modulus
- Elmendorf Tear Strength MD
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|