Custom Resins Nylene® 404 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection from heat
degradation, 404 has high flow characteristics at minimal processing temperatures.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|