Custom Resins Nylene® 721 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Injection molding grade. Nylene 721 is a medium impact modified nylon for fast, easy molding. Parts molded from 721 have good impact strength right out of the mold without post conditioning. Stiffness is near
that of unmodified nylon 6. Cylinder temperatures should be in the 450 - 500ºF range.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|