Custom Resins Nylene® 733 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Injection molding grade. Nylene 733 is a high impact modified nylon suitable for both molding and extrusion. Parts molded from 733 have excellent impact strength right out of the mold without post conditioning. Highlights of Nylene 733 include high stiffness and high strength. Cylinder
temperatures should be in the 500 - 550ºF range.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
|
|
|
|