Custom Resins Nylene® 734 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Injection molding grade. Nylene 734 is the heat stabilized version of 733 which is a high impact modified nylon suitable for both molding and extrusion. In addition to heat stabilization to prevent thermal
degradation, parts molded from 734 have excellent impact strength right out of the mold
without post conditioning. Outstanding features of Nylene 734 include high stiffness and high
strength. Cylinder temperatures should be in the 500 - 550ºF range.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|