Custom Resins Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Film Grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recommended for
flexible packaging where as a film or coating it is used for the outside layer in multi-ply film
constructions. Nylene 609 has excellent melt flow and melt strength properties. Optimum
processing conditions should permit for a melt temperature of 550 - 575ºF at the die.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|