Custom Resins Nylene® 601 Nylon 6, 50% RH, Extrusion Grade
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Extrusion grade. Nylene 601 is the heat stabilized version of 600 which is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications
include wire jacketing and centrifugal casting which require good dielectric properties,
toughness, and fatigue resistance. Optimum processing conditions should provide a melt
temperature of 480 - 500ºF at the die.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|