Custom Resins Nylene® 607 Nylon 6, 50% RH, Extrusion Grade

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Close Analogs:

Data provided by the manufacturer

Key Words: Polyamide 6

Material Notes:
Extrusion grade. Nylene 607 is a very high viscosity extrusion resin having an ASTM relative viscosity of 800. Nylene 607 has excellent structural strength, durability, and physical properties. It has good melt strength and good draw-down properties which promote dimensional control for extrusion of pipe, tubing, film, and sheet. It is particularly recommended for the extrusion of thick slab, large rod stock, and large complex profiles. Optimum processing conditions should permit for a melt temperature of 550 - 575ºF at the die.

Available Properties
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。