Custom Resins Nylene® NX4001 Nylon 6, Extrusion Grade
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Extrusion grade. Nylene NX4001A is a high viscosity, nucleated, nylon 6 extrusion grade resin. Crystallization initiators provide rapid melt set-up in higher speed processing applications. Optimum
processing conditions should provide a melt temperature of 550 - 575ºF at the die.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|