Custom Resins Nylene® NX5703 Nylon 6, Impact Extrusion Grade
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Extrusion grade. Nylene NX5703 is a high residual monomer, medium viscosity resin designed for extrusion applications requiring good flexibility and high strength. NX5703 is ideally suited for
monofilament extrusion such as fish line and netting, sewing thread, and weaving thread.
Optimum processing conditions should provide a melt temperature of 450 - 475ºF at the die.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Flexural Yield Strength
- Izod Impact, Notched
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|