Custom Resins Nylene® NX3024F Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 6
Material Notes: Dry as molded. Nylene NX3024F is a medium viscosity nylon 6 resin suitable for general purpose molding applications. In addition to excellent melt stability and good melt strength, NX3024F has
excellent grease resistance, toughness, resistance to abrasion, and does not absorb food
odors. Nylene NX3024F meets the requirements of FDA regulation 21 CFR 177.1500 for
direct food contact. Optimum processing conditions should provide a melt temperature of 480
- 500ºF at the die.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Flexural Yield Strength
- Izod Impact, Notched
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|