Custom Resins Nylene® 204 (HS), Fast Cycle Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |