Custom Resins Nylene® 7232 MS, 32% Glass/Mineral Reinforced, Low Wear Nylon 6/6
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Description: Nylene® 7232 MS is a 32% glass/mineral reinforced, low wear nylon 6/6. Reinforcement amount: glass - 12%, mineral - 20%, MoS2 - 2%. Information provided by Custom Resins
| Available Properties |
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
|
|
|
|