Custom Resins Nylene® NX4528, Unfilled Nylon 6,6/6
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Description: Nylene® NX 4528 is an unfilled specialty nylon. 4528 is FDA/NSF approved. Information provided by Custom Resins.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Melting Point
|
|
|
|