Custom Resins Nylene® 7250 C HS, 50% Glass Fiber/Ceramic Reinforced, Low Warp, High Stiffness Specialty Nylon
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Nylene® 7250 C HS is a 50% glass fiber/ceramic reinforced, low warp, high stiffness specialty nylon. Information provided by Custom Resins.