Custom Resins Vexel™ E20GF15, 15% Glass Reinforced PET
Subcategory: Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Material Notes: Description: Vexel™ E20GF15 is a 15% glass fiber reinforced, general purpose PET. Information provided by Custom Resins.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|