Custom Resins Naxel™ PC530-112, UV Resistant Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Material Notes: Description: Naxel™ PC530-112 is a high flow, UV resistant polycarbonate. Information provided by Custom Resins.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|