Ashley Polymers Ashlene® PE126WO PET Polyester, 30% Glass Reinforced
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Key Words: Polyethylene Terephthalate; Ashley Polymers, Inc.
Material Notes: PET Polyester with 30% glass reinforcement, flame retardant, natural. Note: Colors will modify properties.Data provided by the manufacturer
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Flammability, UL94
|
|
|
|
| Property Data |