Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Key Words: Polyethylene Terephthalate; Ashley Polymers, Inc.
Material Notes: PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |