Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon
Subcategory: Nylon; Thermoplastic; Nylon, Other
Key Words: Polyamide; Ashley Polymers, Inc.
Material Notes: D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Refractive Index
- Transmission, Visible
- Processing Temperature
|
|
|
|