Ashley Polymers Ashlene® 528LS-33GB Nylon 66, Glass Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; Ashley Polymers, Inc.
Material Notes: General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|