Ashley Polymers Ashlene® 79MGS Nylon 6, 40% Glass Mineral reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 6; Ashley Polymers, Inc.
Material Notes: A 40% glass mineral reinforced Nylon 6 with good dimensional stability, stiffness, sink and warp resistance. Modified for improved surface appearance.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|