Ashley Polymers Ashlene® P126 PBT Polyester, 30% Glass Reinforced
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Key Words: Polybutylene Terephthalate; Ashley Polymers, Inc.
Material Notes: PBT polyester with 30% glass reinforcement.Data provided by the manufacturer