Ashley Polymers Ashlene® 935-40M Nylon 11
Subcategory: Nylon; Thermoplastic; Nylon 11
Key Words: Polyamide 11; Ashley Polymers, Inc.
Material Notes: A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Brittleness Temperature
- Glass Temperature
|
|
|
|