Ashley Polymers Ashlene® L930 Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Key Words: Polyamide 12; Ashley Polymers, Inc.
Material Notes: A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|