Ashley Polymers Ashlene® D926 Nylon 12
Subcategory: Nylon; Thermoplastic; Nylon 12
Key Words: Polyamide 12; Ashley Polymers, Inc.
Material Notes: A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also available with UV stabilizer, designated D926H.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |