Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Key Words: Polyamide 12; Ashley Polymers, Inc.
Material Notes: A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general purpose grade, black.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|