Nabaltec APYRAL® 30X Al(OH)3

 

Material Notes:
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decomposition APYRAL ® does not generate toxic or corrosive gases. In addition, there is a distinct reduction in smoke density. APYRAL ® is effective in the crucial phase of the burning process before the outbreak of a fully developed fire.

APYRAL ® can be used as a flame retardant filler in

  • Thermosets
  • Elastomers
  • Thermoplastics
  • Cable Compounds
  • Technical Rubber Compounds
  • Pressed and cast Plastic Parts
  • Thermal Insulation Foams
  • Glass-fiber reinforced plastics

Available Properties
  • Density
  • Bulk Density
  • Loss On Ignition
  • Particle Size
  • Specific Surface Area
  • Moisture Content
  • Al(OH)3 wt %
  • Cystal Structure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。