Nabaltec NABALOX® NO 325 Ground Alumina
Subcategory: Oxide, Aluminum; Oxide
Material Notes: NABALOX® aluminum oxide has a number of advantages including - low sintering temperature
- wide sintering range
- flexible processing
- high sintered densities high wear and impact resistance
- electrical insulation
- high mechanical strength
- high temperature properties
- dimensional accuracy
- optimized chemical resistance
Refractory Industry, Wear-resistant ceramics
| Available Properties |
- Density
- Bulk Density
- Loss On Ignition
- Particle Size
- Specific Surface Area
- Shrinkage
- Sintering Temperature
- alpha-Al2O3-Content %
|
|
|
|