Ashley Polymers Ashlene® 980LS Nylon 612
Subcategory: Nylon; Thermoplastic; Nylon 612
Key Words: Polyamide 612; Ashley Polymers, Inc.
Material Notes: A general purpose 612 nylon for injection molding, lubricated and heat stabilized. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dissipation Factor
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|