Ashley Polymers Ashlene® 990L-40G Nylon 610, 40% Glass Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 610; Polymer
Key Words: Polyamide 610; Ashley Polymers, Inc.
Material Notes: 40% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-40G, same with heat stabilizer.Data provided by the manufacturer
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|