Ashley Polymers Ashlene® ABS 243
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Ashley Polymers, Inc.
Material Notes: Medium impact, high flow, rigid. Suitable for injection molding of appliances, automotive components, office machines, switch boxes and panels.Data provided by the manufacturer