Ashley Polymers Ashlene® ABS Resin E213B
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Ashley Polymers, Inc.
Material Notes: General purpose, black, utility grade for injection molding with medium gloss.Data provided by the manufacturer
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |