Ashley Polymers Ashlene® 1420B Polycarbonate, 20% Glass Reinforced
Subcategory: Polycarbonate; Thermoplastic; Polymer
Key Words: PC; Ashley Polymers, Inc.
Material Notes: A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties, modified for good impact with increased dimensional stability and overall toughness. 1423B with UV stabilizer.Data provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|